BYNEL™ 50E806
Details:

Anhydride-modified polypropylene resin. Available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylene (PP) resins.


Properties

These values are typical properties and are not intended for use in preparing specifications.   

- Melt Index (g/10min @190°C/21.6 kg)    25

- Melting Point in °C(°F)     140°C (284°F) - ASTM D3418